Typical Technical Parameters |
|
ACID PROOF BRICKS |
|
 |
Particulars |
Class I Bricks |
Class II Bricks |
PHYSICAL PROPERTIES |
|
|
Water absorption, kg/cm2 , Max. |
2 |
4 |
Flexural strength, kg/cm2, Min. |
130 |
90 |
Compressive strength, kg/cm2, Min |
700 |
500 |
CHEMICAL PROPERTIES |
|
|
Resistance to acid |
Loss in weight shall not exceed 1.5% |
Loss in weight shall not exceed 1.5% |
NOTE :
- Data given are typical of machine pressed standard bricks.
- Values of A.P.% and CCS (kg/cm2) are arthmatic mean of individual results.
- Size tolerance ± 1.5% or 2 mm whichever is greater.
- Besides the products listed in the catalogue, we are having sound technical expertise
to meet the customers requirements.
|
|
 |
|